- 密度 [g/cm3]: 1.47
| Physical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Density | 1.47 g/cc | 0.0531 lb/in³ | Silicone Property; Arlon SQA-TMS-024 | ||
| Mechanical Properties | Metric | English | Comments | ||
| Hardness, Shore A | 55 | 55 | Silicone Property; ASTM D2240 | ||
| Tensile Strength | 4.83 MPa | 700 psi | Silicone Property; ASTM D412 | ||
| Elongation at Break | 550 % | 550 % | Silicone Property; ASTM D412 | ||
| Poissons Ratio | 0.50 | 0.50 | Approximately, Silicone Property | ||
| Electrical Properties | Metric | English | Comments | ||
| Volume Resistivity | 3.80e+15 ohm-cm | 3.80e+15 ohm-cm | ASTM D257-99 | ||
| Dielectric Constant | 3.4 @Frequency 1.00e+6 Hz | 3.4 @Frequency 1.00e+6 Hz | Dk, Silicone Property; IPC TM 650-2.5.5.3 | ||
| Dissipation Factor | 0.0040 @Frequency 1.00e+6 Hz | 0.0040 @Frequency 1.00e+6 Hz | Df, Silicone Property; IPC TM 650-2.5.5.3 | ||
| Thermal Properties | Metric | English | Comments | ||
| CTE, linear | 220 µm/m-°C @Temperature 30.0 - 150 °C | 122 µin/in-°F @Temperature 86.0 - 302 °F | Silicone Property; ASTM E 831 | ||
| Thermal Conductivity | 0.400 W/m-K @Temperature 100 °C | 2.78 BTU-in/hr-ft²-°F @Temperature 212 °F | Silicone Property; ASTM E 1530 | ||
| Maximum Service Temperature, Air | 204 °C | 400 °F | |||
| Minimum Service Temperature, Air | -73.3 °C | -100 °F | |||
| Glass Transition Temp, Tg | <= -100 °C | <= -148 °F | Silicone Property; ASTM D3418 | ||
| Processing Properties | Metric | English | Comments | ||
| Cure Time | 15.0 min @Temperature 121 °C | 0.250 hour @Temperature 250 °F | Recommended Cure Cycle | ||
| Shelf Life | 6.00 Month @Temperature 21.1 °C | 6.00 Month @Temperature 70.0 °F | From date of manufacture | ||
| Descriptive Properties | |||||
| Color | Red | ||||