| Availability  | 
 | 
| Filler / Reinforcement  | 
 | 
| Processing Method  | 
 | 
| Physical | Nominal Value | Unit | Test Method | 
| Density | 1.23 | g/cm³ | ISO 1183 | 
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 1.2 | % | |
| Flow | 0.40 | % | |
| Water Absorption | ISO 62 | ||
| Saturation, 23°C | 7.0 | % | |
| Equilibrium, 23°C, 50% RH | 2.3 | % | 
| Mechanical | Nominal Value | Unit | Test Method | 
| Tensile Modulus (23°C) | 6250 | MPa | ISO 527-2 | 
| Tensile Stress (Break, 23°C) | 130 | MPa | ISO 527-2 | 
| Tensile Strain (Break, 23°C) | 3.0 | % | ISO 527-2 | 
| Flexural Modulus (23°C) | 5500 | MPa | ISO 178 | 
| Flexural Strength (23°C) | 180 | MPa | ISO 178 | 
| Impact | Nominal Value | Unit | Test Method | 
| Charpy Notched Impact Strength | ISO 179/eA | ||
| -30°C | 7.0 | kJ/m² | |
| 23°C | 8.0 | kJ/m² | |
| Charpy Unnotched Impact Strength | ISO 179/eU | ||
| -30°C | 40 | kJ/m² | |
| 23°C | 45 | kJ/m² | |
| Notched Izod Impact Strength | ISO 180/1A | ||
| -30°C | 6.0 | kJ/m² | |
| 23°C | 7.0 | kJ/m² | 
| Thermal | Nominal Value | Unit | Test Method | 
| Heat Deflection Temperature | |||
| 0.45 MPa, Unannealed | 250 | °C | ISO 75-2/B | 
| 1.8 MPa, Unannealed | 245 | °C | ISO 75-2/A | 
| Vicat Softening Temperature | 250 | °C | ISO 306/B | 
| Melting Temperature (DSC) | 262 | °C | ISO 3146 | 
| Electrical | Nominal Value | Unit | Test Method | 
| Surface Resistivity | 1.0E+13 | ohm | IEC 60093 | 
| Volume Resistivity | 1.0E+15 | ohm·cm | IEC 60093 | 
| Comparative Tracking Index | 500 | V | IEC 60112 | 
| Flammability | Nominal Value | Unit | Test Method | 
| Flame Rating | UL 94 | ||
| 1.60 mm | HB |  | |
| 3.20 mm | HB |  | |
| Glow Wire Ignition Temperature (2.00 mm) | 650 | °C | IEC 60695-2-13 | 
| Additional Information | Nominal Value | Unit | Test Method | 
| Filler Content | 15 | % | ISO 3451 | 
| Injection | Nominal Value | Unit |  | 
| Drying Temperature | 80.0 | °C | |
| Drying Time | 2.0 | hr | |
| Suggested Max Moisture | 0.20 | % | |
| Suggested Max Regrind | 25 | % | |
| Processing (Melt) Temp | 270 to 300 | °C | |
| Mold Temperature | 50.0 to 110 | °C | |
| Holding Pressure | 50.0 to 100 | MPa | |
| Injection Notes | |||
| Back Pressure: Low | |||