加工/物理特性值(Value)单位(Unit)测试标准(Test Standard)
ASTM数据(ASTM Data)
熔体流动指数(Melt Flow Index)10g/10minASTM D 1238
模具收缩(Mold Shrinkage) (MD)0.0065mm/mmASTM D 955
模具收缩(Mold Shrinkage) (TD)0.0065mm/mmASTM D 955
密度(Density) (73°F)1060kg/m³ASTM D 792
机械性能(机械性能(Mechanical properties))值(Value)单位(Unit)测试标准(Test Standard)
ASTM数据(ASTM Data)
拉伸模量(Tensile Modulus)2233.9MPaASTM D 638
抗拉强度(Tensile Strength) at Yield47.6MPaASTM D 638
抗拉强度(Tensile Strength) at Break41.4MPaASTM D 638
屈服伸长率(Elongation at Yield)3.6%ASTM D 638
断裂伸长率(Elongation at Break)45%ASTM D 638
弯曲弹性模量(弯曲弹性模量(Flexural Modulus))2144.27MPaASTM D 790
抗弯强度(Flexural Strength)69.6MPaASTM D 790
悬臂梁式冲击切口 (1/8 in)0.315kJ/mASTM D 256
悬臂梁式冲击切口 (Low-温度(Temperature))0.123kJ/mASTM D 256
温度(Temperature)-30°CASTM D 256
热性能(热性能(Thermal properties))值(Value)单位(Unit)测试标准(Test Standard)
ASTM数据(ASTM Data)
热膨胀系数(Coefficient of Thermal Expansion) (MD)85.9E-6/KASTM D 696
热膨胀系数(Coefficient of Thermal Expansion) (TD)94.9E-6/KASTM D 696
DTUL @ 66 psi124°CASTM D 648
DTUL @ 264 psi108°CASTM D 648
Vicat 温度(Temperature)141°CASTM D 1525
CharacteristicsProcessingBlow MoldingApplicationsAutomotiveRegional AvailabilityNorth AmericaDisclaimerCopyright M-Base .

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/wuxingbiao/show-102117.html

免责声明: 本文 Noryl BN9003G|(PPE+PS)|SABIC_IP 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4