- 密度 [g/cm3]: 0.6
| Physical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Density | 0.600 g/cc | 0.0217 lb/in³ | |||
| Storage Temperature | 4.00 °C | 39.2 °F | |||
| Mechanical Properties | Metric | English | Comments | ||
| Compressive Strength | 26.2 MPa | 3800 psi | |||
| Adhesive Bond Strength | 10.3 MPa @Temperature 93.0 °C | 1490 psi @Temperature 199 °F | Tensile Lap Shear | ||
| 13.8 MPa @Temperature -55.0 °C | 2000 psi @Temperature -67.0 °F | Lap Shear | |||
| 18.0 MPa @Temperature 25.0 °C | 2610 psi @Temperature 77.0 °F | Tensile Lap Shear | |||
| Thermal Properties | Metric | English | Comments | ||
| Maximum Service Temperature, Air | 149 °C | 300 °F | |||
| Processing Properties | Metric | English | Comments | ||
| Cure Time | 60.0 min @Temperature 82.0 °C | 1.00 hour @Temperature 180 °F | |||
| 7200 - 10100 min @Temperature 25.0 °C | 120 - 168 hour @Temperature 77.0 °F | ||||
| Pot Life | 120 min | 120 min | |||
| Descriptive Properties | |||||
| Consistency | Syntactic | ||||
| Form | 2 parts | ||||
| Mix Ratio, Part A:Part B | 100:31 | ||||
| Peel Strength | Nil | ||||