- 拉伸强度 [MPa]: 1958.0
- 断裂伸长率 [%]: 1034
- 弯曲模量 [MPa]: 290
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 1958 MPa @Temperature 23.0 °C | 284000 psi @Temperature 73.4 °F | 0° |
| Tensile Modulus | 352 GPa @Temperature 23.0 °C | 51100 ksi @Temperature 73.4 °F | 0° |
| Flexural Yield Strength | 1034 MPa | 150000 psi | 0°, Room Temperature |
| Flexural Modulus | 290 GPa | 42100 ksi | 0°, Room Temperature |
| Compressive Yield Strength | 869 MPa | 126000 psi | 0°, Room Temperature |
| Compressive Modulus | 324 GPa | 47000 ksi | 0°, Room Temperature |
| Shear Strength | 80.0 MPa @Temperature 22.0 °C | 11600 psi @Temperature 71.6 °F | 0° |