| Physical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Solids Content | >= 99 % | >= 99 % | 3 hr @ 105°C | ||
| Viscosity Measurement | 20 @Temperature 23.0 °C | 20 @Temperature 73.4 °F | [g/min] Extruding Viscosity (Severs/Press flow; 5mm orifice, @ 43 psi) | ||
| 70 @Temperature 45.0 °C | 70 @Temperature 113 °F | [g/min] Extruding Viscosity (Severs/Press flow; 5mm orifice, @ 43 psi) | |||
| Thermal Properties | Metric | English | Comments | ||
| Maximum Service Temperature, Air | 220 °C | 428 °F | 30 min | ||
| Descriptive Properties | |||||
| Damping Performance: Composite Loss Factor | 0.192 | SAE J 1637, 2 mm thick, 10°C | |||