- 拉伸强度 [MPa]: 12.5
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 90 | 90 | |
| Tensile Strength, Yield | 12.5 MPa | 1810 psi | |
| Elongation at Yield | 510 % | 510 % | |
| 100% Modulus | 0.00501 GPa | 0.726 ksi | |
| 200% Modulus | 0.00671 GPa | 0.973 ksi | |
| 300% Modulus | 0.00786 GPa | 1.14 ksi | |
| Tear Strength | 56.4 kN/m | 322 pli | Die C |
| Processing Properties | Metric | English | Comments |
| Cure Time | 15.0 min @Temperature 155 °C | 0.250 hour @Temperature 311 °F | |