- 拉伸强度 [MPa]: 33.8
| Mechanical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Hardness, Shore A | 65 | 65 | |||
| Tensile Strength, Yield | 33.8 MPa | 4900 psi | |||
| Elongation at Break | 620 % | 620 % | |||
| 300% Modulus | 0.00896 GPa | 1.30 ksi | |||
| Compression Set | 31 % @Temperature 70.0 °C, Time 79200 sec | 31 % @Temperature 158 °F, Time 22.0 hour | |||
| Processing Properties | Metric | English | Comments | ||
| Cure Time | 25.0 min @Temperature 154 °C | 0.417 hour @Temperature 310 °F | |||
| Descriptive Properties | |||||
| 500% Modulus (ksi) | 3 | ||||