- 熔体流动速率 [g/10min]: 0.2
 - 密度 [g/cm3]: 0.92
 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1183-A | 
| ESCR 10% Igepal® | 20 hour | 20 hour | F50; ASTM D1693 | 
| Thickness | 100 microns | 3.94 mil | |
| Melt Flow | 0.20 g/10 min @Load 2.16 kg, Temperature 190 °C  | 0.20 g/10 min @Load 4.76 lb, Temperature 374 °F  | ISO 1133 | 
| Mechanical Properties | Metric | English | Comments | 
| Film Elongation at Break, MD | 330 % | 330 % | ISO 1184 | 
| Film Elongation at Break, TD | 480 % | 480 % | ISO 1184 | 
| Elmendorf Tear Strength MD | 250 g | 250 g | ISO 6283-2 | 
| Elmendorf Tear Strength TD | 500 g | 500 g | ISO 6283-2 | 
| Elmendorf Tear Strength, MD | 2.50 g/micron | 63.5 g/mil | ISO 6283-2 | 
| Elmendorf Tear Strength, TD | 5.00 g/micron | 127 g/mil | ISO 6283-2 | 
| Dart Drop | 6.50 g/micron | 165 g/mil | F50; ISO 7765-A | 
| Dart drop Test | 650 g | 1.43 lb | F50; ISO 7765-A | 
| Film Tensile Strength at Break, MD | 23.0 MPa | 3340 psi | ISO 1184 | 
| Film Tensile Strength at Break, TD | 20.0 MPa | 2900 psi | ISO 1184 | 
| Processing Properties | Metric | English | Comments | 
| Melt Temperature | 220 °C | 428 °F | |
| Blow-up Ratio (BUR) | 2.0 | 2.0 | |