- 密度 [g/cm3]: 8.0
- 热变形温度 [℃]: 150.0
| Physical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Density | 8.00 g/cc | 0.289 lb/in³ | ISO 1183 | ||
| Linear Mold Shrinkage | 0.010 - 0.015 cm/cm | 0.010 - 0.015 in/in | ISO 294-4 | ||
| Mechanical Properties | Metric | English | Comments | ||
| Tensile Strength at Break | 45.0 MPa | 6530 psi | ISO 527-2/50 | ||
| Elongation at Break | 1.0 - 2.0 % | 1.0 - 2.0 % | ISO 527-2/50 | ||
| Tensile Modulus | 5.00 GPa | 725 ksi | ISO 527-2/1 | ||
| Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179 | ||
| Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179 | ||
| Electrical Properties | Metric | English | Comments | ||
| Surface Resistance | <= 1000 ohm | <= 1000 ohm | IEC 60093 | ||
| Thermal Properties | Metric | English | Comments | ||
| Thermal Conductivity | 1.50 - 2.00 W/m-K | 10.4 - 13.9 BTU-in/hr-ft²-°F | ASTM E1461 | ||
| Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | Unannealed; ISO 75-2/B | ||
| Deflection Temperature at 1.8 MPa (264 psi) | 110 °C | 230 °F | Unannealed; ISO 75-2/A | ||
| Processing Properties | Metric | English | Comments | ||
| Melt Temperature | 230 - 280 °C | 446 - 536 °F | |||
| Mold Temperature | 65.0 - 100 °C | 149 - 212 °F | |||
| Drying Temperature | 80.0 °C | 176 °F | |||
| Dry Time | 4.00 hour | 4.00 hour | |||
| Descriptive Properties | |||||
| Appearance | Grey | ||||
| Features | High Specific Gravity | ||||
| Medium Impact Resistance | |||||
| Non-Toxic | |||||
| Forms | Pellets | ||||
| Generic Material | Nylon 12 | ||||
| Generic Name | Polyamide 12 (Nylon 12) | ||||
| Processing Method | Injection Molding | ||||
| Regional Availability | Africa & Middle East | ||||
| Asia Pacific | |||||
| Europe | |||||
| North America | |||||
| South America | |||||
| Uses | Housings | ||||
| Medical/Healthcare Applications | |||||
| Radiation Shielding | |||||
| Weighting & Balancing | |||||