- 拉伸强度 [MPa]: 4.96
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
| Hardness, Shore A | 47 | 47 | Instant; ASTM D2240 |
| Tensile Strength, Yield | 4.96 MPa | 720 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
| 2.34 MPa @Strain 300 % | 340 psi @Strain 300 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 | |
| Elongation at Break | 730 % | 730 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
| Tear Strength | 20.2 kN/m | 115 pli | Die C (graves), 20 in/min; ASTM D624 |
| Compression Set | 20 % | 20 % | Method B, 73°F(23°C), 22 hrs; ASTM D395 |