- 拉伸强度 [MPa]: 5.86
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.890 g/cc | 0.890 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
| Hardness, Shore A | 49 | 49 | 10 Sec; ASTM D2240 |
| 52 | 52 | Instant; ASTM D2240 | |
| Tensile Strength, Yield | 5.86 MPa | 850 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
| 3.59 MPa @Strain 300 % | 520 psi @Strain 300 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 | |
| Elongation at Break | 680 % | 680 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
| Tear Strength | 21.0 kN/m | 120 pli | Die C (graves), 20 in/min; ASTM D624 |