- 密度 [g/cm3]: 0.89
- 透光率 [%]: 90.0
| Physical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Density | 0.890 g/cc | 0.0322 lb/in³ | DIN EN ISO 1183-1:2004 | ||
| Mechanical Properties | Metric | English | Comments | ||
| Hardness, Shore A | 60 | 60 | DIN 53505 / ISO 868 | ||
| Tensile Strength at Break | 8.70 MPa | 1260 psi | Deviating from ISO 37 standard test piece is tested with a traverse speed of 200 mm/min; DIN 53504 / ISO 37 | ||
| Elongation at Break | 720 % | 720 % | Deviating from ISO 37 standard test piece is tested with a traverse speed of 200 mm/min; DIN 53504 / ISO 37 | ||
| Graves Tear Strength | 23.0 kN/m | 131 pli | DIN ISO 34-1 Method B (b) | ||
| Thermal Properties | Metric | English | Comments | ||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | with dynamic stress | ||
| 100 °C | 212 °F | static | |||
| Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |||
| Optical Properties | Metric | English | Comments | ||
| Haze | 10 % | 10 % | ASTM D1003-97 | ||
| Transmission, Visible | 90 % | 90 % | ASTM D1003-97 | ||
| Descriptive Properties | |||||
| Clarity (%) | 95 | ASTM D1003-97 | |||
| Color | Transparent | ||||
| Weather Resistance | 1980 MJ/m2 | DIN EN ISO 4892-2 | |||