| Physical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 | ||
| Mechanical Properties | Metric | English | Comments | ||
| Hardness, Shore A | 61 | 61 | 10 sec; ASTM D2240 | ||
| Tensile Strength at Break | 7.03 MPa | 1020 psi | ASTM D412 | ||
| Elongation at Break | 450 % | 450 % | ASTM D412 | ||
| Tear Strength | 29.8 kN/m | 170 pli | ASTM D412 | ||
| Thermal Properties | Metric | English | Comments | ||
| Flammability, UL94 | HB | HB | |||
| Processing Properties | Metric | English | Comments | ||
| Rear Barrel Temperature | 180 °C | 356 °F | |||
| Middle Barrel Temperature | 190 °C | 374 °F | |||
| Front Barrel Temperature | 200 °C | 392 °F | |||
| Nozzle Temperature | 205 °C | 401 °F | |||
| Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |||
| Drying Temperature | 80.0 °C | 176 °F | |||
| Dry Time | 2 - 4 hour | 2 - 4 hour | |||
| Descriptive Properties | |||||
| Injection Rate | Moderate-Fast | ||||