加工/物理特性值(Value)单位(Unit)测试标准(Test Standard)
ASTM数据(ASTM Data)
熔体流动指数(Melt Flow Index)18g/10minASTM D 1238
模具收缩(Mold Shrinkage) (MD)0.014mm/mmASTM D 955
密度(Density) (73°F)1200kg/m³ASTM D 792
吸水率(Water Absorption) (24hr)0.5%ASTM D 570
流变性能(Rheological properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
熔体体积流动速率(Melt volume-flow rate) (MVR)16cm³/10minISO 1133
温度(Temperature)220°CISO 1133
负载(Load)2.16kgISO 1133
成型收缩(Molding shrinkage) (parallel)1.4%ISO 294-4, 2577
成型收缩(Molding shrinkage) (normal)1.4%ISO 294-4, 2577
机械性能(机械性能(Mechanical properties))值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
拉伸模量(Tensile Modulus)190MPaISO 527-1/-2
屈服应力(Yield stress)14MPaISO 527-1/-2
屈服应变(Yield strain)24%ISO 527-1/-2
断裂拉伸应变(Nominal strain at break)>50%ISO 527-1/-2
Tensile creep modulus (1h)170MPaISO 899-1
Tensile creep modulus (1000h)130MPaISO 899-1
简支梁冲击强度(Charpy impact strength) (+23°C)NkJ/m²ISO 179/1eU
简支梁冲击强度(Charpy impact strength) (-30°C)NkJ/m²ISO 179/1eU
简支梁缺口冲击强度(Charpy notched impact strength) (+23°C)NkJ/m²ISO 179/1eA
简支梁缺口冲击强度(Charpy notched impact strength) (-30°C)140kJ/m²ISO 179/1eA
Tensile notched impact strength (+23°C)200kJ/m²ISO 8256/1
Stress at 10% elongation11MPaISO 527-1/-2
破坏时应变(Strain at break) TPE>300%ISO 527-1/-2
破坏时应变(Stress at break) TPE35MPaISO 527-1/-2
抗拉强度(撕裂强度(Tear strength))180kN/mISO 34-1
Abrasion resistance120mm³ISO 4649
Shore D hardness (15s)51-ISO 868
ASTM数据(ASTM Data)
抗拉强度(Tensile Strength) at Break40MPaASTM D 638
断裂伸长率(Elongation at Break)550%ASTM D 638
弯曲弹性模量(弯曲弹性模量(Flexural Modulus))207MPaASTM D 790
Shore D Hardness55-ASTM D 2240
悬臂梁式冲击切口 (1/8 in)NkJ/mASTM D 256
悬臂梁式冲击切口 (Low-温度(Temperature))0.128kJ/mASTM D 256
温度(Temperature)-40°CASTM D 256
热性能(热性能(Thermal properties))值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
熔化温度(熔化温度(Melting temperature)) (10°C/min)203°CISO 11357-1/-3
玻璃化转变温度(Glass transition temperature) (10°C/min)-20°CISO 11357-1/-2
温度负荷变形(Temp. of deflection under load) (1.80 MPa)45°CISO 75-1/-2
温度负荷变形(Temp. of deflection under load) (0.45 MPa)65°CISO 75-1/-2
维卡软化温度(50℃/ h的50N)Vicat softening temperature75°CISO 306
COEFF线性热(Coeff. of linear therm. expansion) (parallel)230E-6/KISO 11359-1/-2
COEFF线性热(Coeff. of linear therm. expansion) (normal)230E-6/KISO 11359-1/-2
燃烧性(球压痕硬度(Burning behav)). at 1.5 mm nom. thickn.HBclassIEC 60695-11-10
厚度测试(Thickness tested)1.5mmIEC 60695-11-10
UL 识别(recognition)UL--
燃烧性(球压痕硬度(Burning behav)). at thickness hHBclassIEC 60695-11-10
厚度测试(Thickness tested)3.0mmIEC 60695-11-10
UL 识别(recognition)UL--
Oxygen index21%ISO 4589-1/-2
ASTM数据(ASTM Data)
UL 94 阻燃等级(Flame rating)HB-UL 94
厚度测试(Thickness tested)1.5mm-
热膨胀系数(Coefficient of Thermal Expansion) (MD)187E-6/KASTM D 696
热膨胀系数(Coefficient of Thermal Expansion) (TD)171E-6/KASTM D 696
DTUL @ 66 psi90°CASTM D 648
DTUL @ 264 psi49°CASTM D 648
熔化温度(Melting 温度(Temperature))203°CASTM D 3418
电气性能(Electrical properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
相对介电常数(Relative permittivity) (100Hz)4.9-IEC 60250
相对介电常数(Relative permittivity) (1MHz)4.6-IEC 60250
耗散因数(耗散因数(Dissipation factor)) (100Hz)90E-4IEC 60250
耗散因数(耗散因数(Dissipation factor)) (1MHz)375E-4IEC 60250
体积电阻率(Volume resistivity)>1E13Ohm*mIEC 60093
表面电阻率(Surface resistivity)>1E15OhmIEC 60093
电气强度(Electric strength)20kV/mmIEC 60243-1
相比漏电起痕指数(Comparative tracking index)600-IEC 60112
ASTM数据(ASTM Data)
绝缘强度(Dielectric Strength) (Short Time)17.3kV/mmASTM D 149
耗散因数(Dissipation Factor) (1 MHz)0.04-ASTM D 150
介电常数(Dielectric Constant) (1 MHz)4.5-ASTM D 150
其他属性(Other properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
吸水率(Water absorption)0.6%Sim. to ISO 62
吸湿性(Humidity absorption)0.2%Sim. to ISO 62
密度(Density)1190kg/m³ISO 1183
流变计算属性(Rheological calculation properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
密度(Density) of melt1040kg/m³-
熔体热导率(Thermal conductivity of melt)0.19W/(m K)-
规格的热容融化(Spec. heat capacity of melt)2110J/(kg K)-
Eff. thermal diffusivity5.44E-8m²/s-
喷射温度(Ejection temperature)125°C-
DiagramsEng.Oil, ISP (140°C)
ISO 1817 Liquid C) (23°C)
ISO 1817 Liquid 4) (23°C)
ISO 1817 Liquid F) (23°C)
ISO 1817 Liquid F) (90°C)
ISO 1817 Liquid F) (>90°C)
Salt solutions
4 Brake fluid (130°C)
.

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/wuxingbiao/show-103515.html

免责声明: 本文 Hytrel® 5526|TPC|DuPont 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4