- 拉伸强度 [MPa]: 22.1
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.24 g/cc | 1.24 g/cc | |
| Mooney Viscosity | 17 @Temperature 121 °C | 17 @Temperature 250 °F | |
| Mechanical Properties | Metric | English | Comments |
| Hardness, Shore A | 56 | 56 | |
| Tensile Strength, Yield | 22.1 MPa | 3200 psi | |
| Elongation at Yield | 600 % | 600 % | |
| 100% Modulus | 0.00155 GPa | 0.225 ksi | |
| 300% Modulus | 0.00276 GPa | 0.400 ksi | |
| Tear Strength | 25.8 kN/m | 147 pli | Graves |
| Compression Set | 22 % | 22 % | Method B |
| Processing Properties | Metric | English | Comments |
| Cure Time | 90.0 min @Temperature 142 °C | 1.50 hour @Temperature 287 °F | |