- 拉伸强度 [MPa]: 15.0
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 83 | 83 | |
| Tensile Strength, Yield | 15.0 MPa | 2180 psi | |
| Elongation at Yield | 125 % | 125 % | |
| 100% Modulus | 0.00483 GPa | 0.700 ksi | |
| Tear Strength | 13.7 kN/m | 78.2 pli | Die C |
| Compression Set | 10.6 % @Temperature 70.0 °C, Time 79200 sec | 10.6 % @Temperature 158 °F, Time 22.0 hour | |
| Processing Properties | Metric | English | Comments |
| Cure Time | 4.90 min @Temperature 177 °C | 0.0817 hour @Temperature 350 °F | |