- 拉伸强度 [MPa]: 21.0
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 66 | 66 | |
| Tensile Strength, Yield | 21.0 MPa | 3050 psi | |
| Elongation at Yield | 421 % | 421 % | |
| 100% Modulus | 0.007302 GPa | 1.059 ksi | |
| 200% Modulus | 0.01347 GPa | 1.953 ksi | |
| 300% Modulus | 0.01677 GPa | 2.433 ksi | |
| Tear Strength | 49.9 kN/m | 285 pli | Die C |
| Compression Set | 55 % @Temperature 70.0 °C, Time 79200 sec | 55 % @Temperature 158 °F, Time 22.0 hour | |
| Processing Properties | Metric | English | Comments |
| Cure Time | 33.0 min @Temperature 154 °C | 0.550 hour @Temperature 310 °F | Press cured |