- 熔体流动速率 [g/10min]: 2.3
 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 0.916 g/cc | 0.916 g/cc | ASTM D1505/D792 | 
| Thickness | 25.0 microns | 0.984 mil | |
| Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C  | 2.3 g/10 min @Load 4.76 lb, Temperature 374 °F  | ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
| Film Elongation at Break, MD | 950 % | 950 % | ASTM D882 | 
| Film Elongation at Break, TD | 1180 % | 1180 % | ASTM D882 | 
| Elmendorf Tear Strength MD | 270 g | 270 g | gF; ASTM D1922 | 
| Elmendorf Tear Strength TD | 500 g | 500 g | gF; ASTM D1922 | 
| Dart drop Test | 170 g | 0.375 lb | g/F50; ASTM D1709 | 
| Film Tensile Strength at Break, MD | 40.0 MPa | 5800 psi | ASTM D882 | 
| Film Tensile Strength at Break, TD | 40.0 MPa | 5800 psi | ASTM D882 | 
| 1% Secant Modulus, MD | 170 MPa | 24700 psi | ASTM D882 | 
| 1% Secant Modulus, TD | 180 MPa | 26100 psi | ASTM D882 | 
| Optical Properties | Metric | English | Comments | 
| Haze | 35 % | 35 % | ASTM D1003 | 
| Gloss | 49 % | 49 % | 60°; ASTM D2457 | 