| Physical Properties | Metric | English | Comments | ||
|---|---|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 | ||
| Mechanical Properties | Metric | English | Comments | ||
| Hardness, Shore A | 65 | 65 | 10 sec; ASTM D2240 | ||
| Tensile Strength at Break | 16.0 MPa | 2320 psi | ASTM D412 | ||
| Elongation at Break | 500 % | 500 % | ASTM D412 | ||
| Tear Strength | 29.8 kN/m | 170 pli | ASTM D412 | ||
| Taber Abrasion, mg/1000 Cycles | 21 | 21 | ASTM D1044 | ||
| Compression Set | 12 % @Temperature 22.8 °C, Time 79200 sec | 12 % @Temperature 73.0 °F, Time 22.0 hour | |||
| 70 % @Temperature 120 °C, Time 79200 sec | 70 % @Temperature 248 °F, Time 22.0 hour | ||||
| Tensile Set | 6.0 % | 6.0 % | 100; ASTM D412 | ||
| 20 % | 20 % | 300; ASTM D412 | |||
| 24 % | 24 % | ASTM D412 | |||
| 24 % | 24 % | At Break; ASTM D412 | |||
| Electrical Properties | Metric | English | Comments | ||
| Dielectric Constant | 4.13 | 4.13 | |||
| Dielectric Strength | 18.0 kV/mm | 457 kV/in | |||
| 18.0 kV/mm @Frequency 100 Hz | 457 kV/in @Frequency 100 Hz | ||||
| Processing Properties | Metric | English | Comments | ||
| Rear Barrel Temperature | 180 °C | 356 °F | |||
| Middle Barrel Temperature | 190 °C | 374 °F | |||
| Front Barrel Temperature | 200 °C | 392 °F | |||
| Nozzle Temperature | 205 °C | 401 °F | |||
| Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |||
| Drying Temperature | 80.0 °C | 176 °F | |||
| Dry Time | 2 - 4 hour | 2 - 4 hour | |||
| Descriptive Properties | |||||
| Injection Rate | Fast | ||||