- 拉伸强度 [MPa]: 6.76
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.890 g/cc | 0.890 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
| Hardness, Shore A | 57 | 57 | 10 Sec; ASTM D2240 |
| 62 | 62 | Instant; ASTM D2240 | |
| Tensile Strength, Yield | 6.76 MPa | 980 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
| 4.48 MPa @Strain 300 % | 650 psi @Strain 300 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 | |
| Elongation at Break | 640 % | 640 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
| Tear Strength | 24.5 kN/m | 140 pli | Die C (graves), 20 in/min; ASTM D624 |